Troubleshooting

Why does my weld have sugaring (stainless)?

Quick answer

Sugaring (stainless) is caused by back side of the stainless weld oxidising from no shielding. The fix: purge the back of the joint with argon or use a backing flux paste.

· · Technical guidance compiled from trade practice and manufacturer data; our source-verification program is in progress — see our editorial policy.

Root causes

Back side of the stainless weld oxidising from no shielding.

The fix sequence

  • purge the back of the joint with argon or use a backing flux paste
  • Change one variable at a time and re-test on scrap
  • Re-inspect the finished bead — chisel, brush, look

When to grind it out

Structural or pressure work with visible defects: grind back to sound metal and re-weld — never 'cap over' a defect and hope. For non-critical jobs, judge honestly: a cosmetic defect is a learning note; a fusion or crack defect is a redo.