Can you laser welding 4130 chromoly?

Quick answer

Yes — production tube work, growing. Laser on 4130 chromoly: match technique to the material; filler ER80S-D2, or ER70S-2 for less critical tube work.

· · Technical guidance compiled from trade practice and manufacturer data; our source-verification program is in progress — see our editorial policy.

The verdict and why

Production tube work, growing. Roll-cage and motorsport tube in Australia: preheat 150–200°C on thick sections and follow the rulebook for post-weld conditioning

Watch-outs

  • acetone wipe, clean tungsten, tight fit-up
  • Prep: acetone wipe, clean tungsten, tight fit-up